ER 347 Wire
400.00 - 450.00 INR/Kilograms
Product Details:
X
ER 347 Wire Price And Quantity
- 100 Kilograms
- 400.00 - 450.00 INR/Kilograms
ER 347 Wire Trade Information
- 20 Kilograms Per Month
- 4 Week
Product Description
AWS Spec: 5.9
AWS Class: ER 347