Superarc EH14 Wire
120.00 - 150.00 INR/Kilograms
Product Details:
X
Superarc EH14 Wire Price And Quantity
- 500 Kilograms
- 120.00 - 150.00 INR/Kilograms
Superarc EH14 Wire Trade Information
- 20 Kilograms Per Month
- 4 Week
Product Description
AWS Class: 5.17 EH14
Moderate carbon, High manganese and Low silicon SAW wire for welding of carbon steels requiring impact toughness upto -40C